Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 1.07e-14 bar @Temperature 1370 °C |
8.00e-12 torr @Temperature 2500 °F |
|
Zircar Zirconia ZYK-15 Zirconia Cloth Insulation Zirconia Cloth Type ZYK-15 is a tricot knit cloth nominally 0.012” thick composed of yttria stabilized zirconia fibers. This material offers extreme temperature and chemical resistance in a flexibl.. |
|||
Vapor Pressure | 1.07e-14 bar @Temperature 2498 °C |
8.00e-12 torr @Temperature 4528 °F |
|
Zircar Zirconia ZYW-15 Zirconia Cloth Insulation Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo.. |
|||
Vapor Pressure | 1.07e-14 bar @Temperature 1370 °C |
8.00e-12 torr @Temperature 2500 °F |
|
Zircar Zirconia ZYF-100 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Vapor Pressure | 1.07e-14 bar @Temperature 1370 °C |
8.00e-12 torr @Temperature 2500 °F |
|
Zircar Zirconia ZYF-150 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Vapor Pressure | 1.07e-14 bar @Temperature 1370 °C |
8.00e-12 torr @Temperature 2500 °F |
|
Zircar Zirconia ZYF-50 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Vapor Pressure | 1.07e-14 bar @Temperature 1370 °C |
8.00e-12 torr @Temperature 2500 °F |
|
Zircar Zirconia ZYK-15 Zirconia Cloth Insulation Zirconia Cloth Type ZYK-15 is a tricot knit cloth nominally 0.012” thick composed of yttria stabilized zirconia fibers. This material offers extreme temperature and chemical resistance in a flexibl.. |
|||
Vapor Pressure | 1.07e-14 bar @Temperature 2498 °C |
8.00e-12 torr @Temperature 4528 °F |
|
Zircar Zirconia ZYW-15 Zirconia Cloth Insulation Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo.. |
|||
Vapor Pressure | 1.07e-14 bar @Temperature 2498 °C |
8.00e-12 torr @Temperature 4528 °F |
|
Zircar Zirconia ZYW-30A Zirconia Cloth Insulation Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo.. |
|||
Vapor Pressure | 1.07e-14 bar @Temperature 1370 °C |
8.00e-12 torr @Temperature 2500 °F |
|
Zircar Zirconia ZYF-100 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Vapor Pressure | 1.07e-14 bar @Temperature 1370 °C |
8.00e-12 torr @Temperature 2500 °F |
|
Zircar Zirconia ZYF-150 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Vapor Pressure | 1.07e-14 bar @Temperature 1370 °C |
8.00e-12 torr @Temperature 2500 °F |
|
Zircar Zirconia ZYF-50 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Vapor Pressure | 1.07e-14 bar @Temperature 2498 °C |
8.00e-12 torr @Temperature 4528 °F |
|
Zircar Zirconia ZYW-30A Zirconia Cloth Insulation Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo.. |