Vapor Pressure 1.07e-14 bar

@Temperature 1370 °C
8.00e-12 torr

@Temperature 2500 °F
Zircar Zirconia ZYK-15 Zirconia Cloth Insulation
Zirconia Cloth Type ZYK-15 is a tricot knit cloth nominally 0.012” thick composed of yttria stabilized zirconia fibers. This material offers extreme temperature and chemical resistance in a flexibl..
Vapor Pressure 1.07e-14 bar

@Temperature 2498 °C
8.00e-12 torr

@Temperature 4528 °F
Zircar Zirconia ZYW-15 Zirconia Cloth Insulation
Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo..
Vapor Pressure 1.07e-14 bar

@Temperature 1370 °C
8.00e-12 torr

@Temperature 2500 °F
Zircar Zirconia ZYF-100 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Vapor Pressure 1.07e-14 bar

@Temperature 1370 °C
8.00e-12 torr

@Temperature 2500 °F
Zircar Zirconia ZYF-150 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Vapor Pressure 1.07e-14 bar

@Temperature 1370 °C
8.00e-12 torr

@Temperature 2500 °F
Zircar Zirconia ZYF-50 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Vapor Pressure 1.07e-14 bar

@Temperature 1370 °C
8.00e-12 torr

@Temperature 2500 °F
Zircar Zirconia ZYK-15 Zirconia Cloth Insulation
Zirconia Cloth Type ZYK-15 is a tricot knit cloth nominally 0.012” thick composed of yttria stabilized zirconia fibers. This material offers extreme temperature and chemical resistance in a flexibl..
Vapor Pressure 1.07e-14 bar

@Temperature 2498 °C
8.00e-12 torr

@Temperature 4528 °F
Zircar Zirconia ZYW-15 Zirconia Cloth Insulation
Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo..
Vapor Pressure 1.07e-14 bar

@Temperature 2498 °C
8.00e-12 torr

@Temperature 4528 °F
Zircar Zirconia ZYW-30A Zirconia Cloth Insulation
Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo..
Vapor Pressure 1.07e-14 bar

@Temperature 1370 °C
8.00e-12 torr

@Temperature 2500 °F
Zircar Zirconia ZYF-100 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Vapor Pressure 1.07e-14 bar

@Temperature 1370 °C
8.00e-12 torr

@Temperature 2500 °F
Zircar Zirconia ZYF-150 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Vapor Pressure 1.07e-14 bar

@Temperature 1370 °C
8.00e-12 torr

@Temperature 2500 °F
Zircar Zirconia ZYF-50 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Vapor Pressure 1.07e-14 bar

@Temperature 2498 °C
8.00e-12 torr

@Temperature 4528 °F
Zircar Zirconia ZYW-30A Zirconia Cloth Insulation
Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo..