Physical Properties Metric English Comments
Vapor Pressure 0.685 bar
514 torr
Average value: 0.685 bar Grade Count:9
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Vapor Pressure 0.685 bar

@Temperature 25.0 °C
514 torr

@Temperature 77.0 °F
BASF Styropor® F 215 N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing a uniformly distributed ?ame retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foams.Applications: Blocks, insula..
Vapor Pressure 0.685 bar

@Temperature 25.0 °C
514 torr

@Temperature 77.0 °F
BASF Styropor® F 315-N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkageApplicati..
Vapor Pressure 0.685 bar

@Temperature 25.0 °C
514 torr

@Temperature 77.0 °F
BASF Styropor® F 395 -N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat..
Vapor Pressure 0.685 bar

@Temperature 25.0 °C
514 torr

@Temperature 77.0 °F
BASF Styropor® P 326 M Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded parts with very good mechanical ..
Vapor Pressure 0.685 bar

@Temperature 25.0 °C
514 torr

@Temperature 77.0 °F
BASF Styropor® P 570 Expandable Polystyrene Additive
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: For the production of expanded particles as a filling material ..
Vapor Pressure 0.685 bar

@Temperature 25.0 °C
514 torr

@Temperature 77.0 °F
BASF Styropor® F 295-N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkageApplicati..
Vapor Pressure 0.685 bar

@Temperature 25.0 °C
514 torr

@Temperature 77.0 °F
BASF Styropor® F 495-N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat..
Vapor Pressure 0.685 bar

@Temperature 25.0 °C
514 torr

@Temperature 77.0 °F
BASF Styropor® P 326 C Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded partsInformation provided by BAS..
Vapor Pressure 0.685 bar

@Temperature 25.0 °C
514 torr

@Temperature 77.0 °F
BASF Styropor® P 426 Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Thin-walled molded parts.Information pr..