Material Notes:
Description: Expandable polystyrene (EPS) containing a uniformly distributed ?ame retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foams.Applications: Blocks, insulating panels, footfall insulating panels.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
Density 0.00310 g/cc
0.000112 lb/in³
Vapor (Heavier than air)
1.02 - 1.05 g/cc
0.0368 - 0.0379 lb/in³
Bead Size 1.00 - 2.00 mm
0.0394 - 0.0787 in
Vapor Pressure 0.685 bar

@Temperature 25.0 °C
514 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Softening Point 70.0 °C
158 °F
approx
Decomposition Temperature >= 220 °C
>= 428 °F
Flash Point >= -56.0 °C
>= -68.8 °F
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Color White
Commercial Status Europe
Ignition Temperature 285°C
DIN 51794
Sieve Analysis <0.8 mm
max 4%
>2.1 mm
max 2%
0.8 - 2.1 mm
max 94%