Physical Properties | Metric | English | Comments |
---|---|---|---|
Neck In | 5.08 cm @Temperature 280 °C |
2.00 in @Temperature 536 °F |
164 ft/min, constant output at 35 rpm; ExxonMobil Method |
ExxonMobil Escor™ 5000 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5000 is primarily intended for extrusion coating, coextrusion coating, extrusion lamination. Very good adhesion to polar substrates, aluminum foil, metalized films, papers.. |
|||
Neck In | 5.08 cm @Temperature 280 °C |
2.00 in @Temperature 536 °F |
164 ft/min, constant output at 35 rpm; ExxonMobil Method |
ExxonMobil Escor™ 5020 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5020 is primarily intended for extrusion coating and coextrusion coating. Very good adhesion to polar substrates, aluminum foil, metalized films, papers, iron, steel and g.. |
|||
Neck In | 5.08 cm @Temperature 280 °C |
2.00 in @Temperature 536 °F |
328 ft/min, constant output at 35 rpm; ExxonMobil Method |
ExxonMobil Escor™ 6000 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 6000 is primarily intended for extrusion coating and coextrusion coating. Escor 6000 is the high draw down version of Escor 5000. Very low coating weight achievable at hig.. |