Physical Properties Metric English Comments
Neck In 6.86 cm

@Temperature 280 °C
2.70 in

@Temperature 536 °F
328 ft/min, constant output at 35 rpm; ExxonMobil Method
ExxonMobil Escor™ 5110 ExCo Ethylene Acrylic Acid Copolymer Resin
Product Description: Escor 5110 is primarily intended for high speed, low coating weight extrusion coating and extrusion lamination. Excellent adhesion to polar substrates, aluminum foil, polyamide ..
Neck In 6.86 cm

@Temperature 280 °C
2.70 in

@Temperature 536 °F
164 ft/min, constant output at 35 rpm; ExxonMobil Method
ExxonMobil Escor™ 6000 ExCo Ethylene Acrylic Acid Copolymer Resin
Product Description: Escor 6000 is primarily intended for extrusion coating and coextrusion coating. Escor 6000 is the high draw down version of Escor 5000. Very low coating weight achievable at hig..