Physical Properties | Metric | English | Comments |
---|---|---|---|
Neck In | 8.64 cm @Temperature 230 °C |
3.40 in @Temperature 446 °F |
656 ft/min, constant output at 35 rpm; ExxonMobil Method |
ExxonMobil Escorene™ FL 01418 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 01418 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. FL 01418 is an excellent sealing materi.. |