Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.000100 - 0.000800 g/m²/day @Temperature 38.0 - 38.0 °C |
0.00000644 - 0.0000515 g/100 in²/day @Temperature 100 - 100 °F |
Average value: 0.000343 g/m²/day Grade Count:3 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Water Vapor Transmission | 0.000100 g/m²/day @Temperature 38.0 °C |
0.00000644 g/100 in²/day @Temperature 100 °F |
90% RH; ISO 15106-3 |
Topas Advanced Polymers TOPAS® 5013F-04 Cyclic Olefin Copolymer (COC) TOPAS® 5013F-04 is a high temperature film extrusion grade for blends. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity .. |