Polymer Property : Water Vapor Transmission = 0.000100 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 0.000100 - 0.000800 g/m²/day

@Temperature 38.0 - 38.0 °C
0.00000644 - 0.0000515 g/100 in²/day

@Temperature 100 - 100 °F
Average value: 0.000343 g/m²/day Grade Count:3
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Water Vapor Transmission 0.000100 g/m²/day

@Temperature 38.0 °C
0.00000644 g/100 in²/day

@Temperature 100 °F
90% RH; ISO 15106-3
Topas Advanced Polymers TOPAS® 5013F-04 Cyclic Olefin Copolymer (COC)
TOPAS® 5013F-04 is a high temperature film extrusion grade for blends. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity ..