Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 1.70 g/m²/day | 0.109 g/100 in²/day | 38°C, 90%RH for 24 Hours; ASTM E96 |
UBE UPILEX 25S (25 micron) Polyimide Film Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries.. |
|||
Water Vapor Transmission | 1.70 - 17.5 g/m²/day | 0.109 - 1.13 g/100 in²/day | Average value: 5.41 g/m²/day Grade Count:9 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |