Polymer Property : Water Vapor Transmission = 1.70 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 1.70 g/m²/day
0.109 g/100 in²/day
38°C, 90%RH for 24 Hours; ASTM E96
UBE UPILEX 25S (25 micron) Polyimide Film
Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries..
Water Vapor Transmission 1.70 - 17.5 g/m²/day
0.109 - 1.13 g/100 in²/day
Average value: 5.41 g/m²/day Grade Count:9
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..