Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.390 g/m²/day | 0.0251 g/100 in²/day | 38°C, 90% RH; ExxonMobil Method |
ExxonMobil Metallyte® 50 TSPM OPP Film Product Description: A high barrier, non-sealable OPP film with one-side metalized a one-side treated. TSP< is designed for use as the inner web of a cold seal lamination or as the center web of a t.. |
|||
Water Vapor Transmission | 0.390 g/m²/day | 0.0251 g/100 in²/day | ASTM E96-66 |
3M Weatherban™ 5354 Sealant Tape 3M™ Weatherban™ Sealant Tape 5354 is a high tack extruded synthetic rubber, non-curing sealant in tape form.It can be used to seal between glass, metal, wood and many plastics.Easy to compress and.. |