Water Vapor Transmission 10.0 g/m²/day
0.644 g/100 in²/day
LG Chemical LUTENE FB0300 LDPE Blown Film Grade
Description: LUTENE FB0300 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of heavy duty sacks and pallet shrink films. LUTENE FB0300 have the e..
Water Vapor Transmission 10.0 g/m²/day
0.644 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
EMS-Grivory Grivory® FG 34 NL nat 6023 PA6
Product description: Grilon FG 34 NL natural 6023 is a modified, medium viscosity polyamide 6. Grilon FG 34 NL natural 6023 exhibits following improvements compared to a PA 6: Better gas barrier pro..
Water Vapor Transmission 10.0 g/m²/day
0.644 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
EMS-Grivory Grivory® FG 40 NL nat 6018 PA6
Information provided by EMS Grivory
Water Vapor Transmission 10.0 g/m²/day
0.644 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
EMS-Grivory Grivory® FG 40 NL nat 6021 PA6
Product description: Grilon FG 40 NL natural 6021 is a modified, high viscosity polyamide 6. As a result of the modification in comparison to conventional polyamide 6 Grilon FG40 NL natural 6021 off..
Water Vapor Transmission 10.0 g/m²/day
0.644 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
EMS-Grivory Grivory® FG 40 NL nat 6025 PA6
Product description: Grilon FG 40 NL natural 6025 is a modified, high viscosity polyamide 6. Compared to conventional polyamide 6 Grilon FG40 NL natural 6025 offers the following improvements:Better..
Water Vapor Transmission 10.0 g/m²/day
0.644 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
EMS-Grivory Grivory® FG 47 NL nat 6028 PA6
Product description: Grilon FG 47 NL natural 6028 is a modified, high viscosity Polyamide 6, which contains also slip and nucleating agents. Grilon FG 47 NL natural 6028 shows following improvements..
Water Vapor Transmission 10.0 g/m²/day
0.644 g/100 in²/day
ASTM F 1249
BASF Ultradur B 4500 PBT
Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660.