Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 100 g/m²/day | 6.44 g/100 in²/day | 104°F (40°C) / 90%RH; ASTM E96 |
Honeywell Oxyshieldâ„¢ BOEB Biaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshieldâ„¢ BOEB is a 0.60 mil (15 micron) biaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relative humidity. T.. |
|||
Water Vapor Transmission | 100 - 150 g/m²/day | 6.44 - 9.66 g/100 in²/day | DIN EN 12086 |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Water Vapor Transmission | 100 - 150 g/m²/day | 6.44 - 9.66 g/100 in²/day | DIN EN 12086 |
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m.. |
|||
Water Vapor Transmission | 100 - 200 g/m²/day | 6.44 - 12.9 g/100 in²/day | DIN EN 12086 |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Water Vapor Transmission | 100 - 150 g/m²/day | 6.44 - 9.66 g/100 in²/day | DIN EN 12086 |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |