Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 25.0 g/m²/day | 1.61 g/100 in²/day | ASTM 1249 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Water Vapor Transmission | 25.0 g/m²/day | 1.61 g/100 in²/day | ASTM 1249 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |
|||
Water Vapor Transmission | 25.0 g/m²/day | 1.61 g/100 in²/day | ASTM F1249 |
Eastman Embrace LV Copolyester for Shrink Film Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo.. |
|||
Water Vapor Transmission | 25.0 g/m²/day | 1.61 g/100 in²/day | 85% RH |
BASF Ultramid® C40 LN 07 0.04 mm Blown Film Cold Air Information provided by BASF |
|||
Water Vapor Transmission | 25.0 g/m²/day | 1.61 g/100 in²/day | ASTM 1249 |
DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 50 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film. Clysar® EZS is a high slip version of EZ. Used where a premium product appearance .. |