DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyolefin , Polyolefin, Film Grade , Polyolefin, Film Grade (Polyolefin)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film. Clysar® EZS is a high slip version of EZ. Used where a premium product appearance is required. Excellent optics, clean shrink appearance, and strong, durable seals are obtained on shadow boxes, irregular shapes, and general purpose overwrapping under a wide range of operating conditions.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.630 cc-mm/m²-24hr-atm
1.60 cc-mil/100 in²-24hr-atm
ASTM 1249
Water Vapor Transmission 25.0 g/m²/day
1.61 g/100 in²/day
ASTM 1249
Oxygen Transmission 160 cc-mm/m²-24hr-atm
406 cc-mil/100 in²-24hr-atm
or 6400 cc/m²-24hr-atm for the film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 125 %
125 %
Average; ASTM D882
Modulus of Elasticity 0.440 GPa
63.8 ksi
(stiffness), ASTM D882
Coefficient of Friction, Dynamic 0.30
0.30
ASTM D1894
Elmendorf Tear Strength MD 24 g
24 g
Orientation not specified; ASTM D1922
Seal Strength 2300 g/25 mm
2300 g/in
F-88-68(73)
Film Tensile Strength at Break, MD 69.0 MPa
10000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 2.1 %
2.1 %
Gloss 145 %
145 %