Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 28.0 g/m²/day | 1.80 g/100 in²/day | 85% RH |
BASF Ultramid® B36 LN 0.04 mm Cast Film Cold Chillroll Product comes in 2-2.5 mm round pellets.Information provided by BASF |
|||
Water Vapor Transmission | 28.0 g/m²/day @Temperature 38.0 °C |
1.80 g/100 in²/day @Temperature 100 °F |
90% RH; 1 µm Coating on BOPP |
Solvay Specialty Polymers Diofan® A 036 Polyvinylidene Chloride (PVDC)
(discontinued **) DIOFAN® A 036 is a PVDC latex used as a flexible under layer for coating on paper and cardboard, to be covered with an appropriate topcoat.Additional Information: PROCESSING - DRYING - DIOFAN® A 0.. |