Physical Properties Metric English Comments
Water Vapor Transmission 6.60 g/m²/day
0.425 g/100 in²/day
ASTM F372
LyondellBasell Petrothene® LP510300 High Density Polyethylene
ApplicationsPETROTHENE LLP 5103-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. It is r..