Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 7.80 g/m²/day | 0.502 g/100 in²/day | 100°F (37.8°C) / 100%RH; ASTM F1249 |
Honeywell Halar® High Performance E-CTFE Film
(discontinued **) Description: Halar® is a high performance Ethylene-Chlorotrifluoroethylene (E-CTFE) film with excellent mechanical, electrical and release properties. It is non-flammable, and has outstanding chem.. |
|||
Water Vapor Transmission | 7.80 g/m²/day | 0.502 g/100 in²/day | ASTM E96 |
LyondellBasell Petrothene® NA217000 Low Density Polyethylene ApplicationsPETROTHENE NA 217-000 is a high speed, lightweight coating resin for use with paper, films and other base stocks. This resin can yield coating weights down to 3.5 lbs/ream at line speed.. |