Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 6.20 - 14.0 cc/m²/day | 0.399 - 0.902 cc/100 in²/day | 77°F / 0% / RH; ASTM D3985 |
Honeywell Capran® K Coated Nylon Film
(discontinued **) Description: Capran® K is a PVdc coated nylon 6 film designed for food packaging applications where longer shelf life is required. This film exhibits good clarity, gloss, toughness, thermoformabil.. |