Oxygen Transmission Rate 50.0 cc/m²/day
3.22 cc/100 in²/day
0% RH,23°C
UBE 1024FD-1 Nylon 6 Film
Description: T-die cast film of 25µm in thicknessInformation provided by UBE.
Oxygen Transmission Rate 50.0 cc/m²/day
3.22 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® F 47 H NL nat 6020 PA6
Product description: Grilon F 47 HNL natural 6020 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good mechanical propertiesGood barrier against oils and fa..
Oxygen Transmission Rate 50.0 cc/m²/day
3.22 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® F 40 NL PA6
Product description: Grilon F 40 NL natural 6018 is a nucleated and lubricated high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGoo..
Oxygen Transmission Rate 50.0 cc/m²/day
3.22 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® F 47 NL nat 6028 PA6
Product description: Grilon F 47 NL natural 6028 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGood barrier agai..
Oxygen Transmission Rate 50.0 cc/m²/day
3.22 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® F 50 nat 6368 PA6
Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro..