EMS-Grivory Grivory® F 40 NL PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® F 40 NL PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon F 40 NL natural 6018 is a nucleated and lubricated high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGood barrier against oils and fatsGood optical properties Application examples: Grilon F 40 NL natural 6018 is suitable for the production of mono and co-extruded blown and cast films. Barrier layer in multi-layer films for food packaging, mostly used as vacuum bags (meat, fish, cheese) and thermoformed pouches or sausage casings.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 9.0 %
9.0 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Water Vapor Transmission 15.0 g/m²/day
0.966 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
Oxygen Transmission Rate 25.0 cc/m²/day
1.61 cc/100 in²/day
23°C/0%r.h.; DIS 15105-1/-2
50.0 cc/m²/day
3.22 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
Carbon Dioxide Transmission 80.0 cc-mm/m²-24hr-atm
203 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
250 cc-mm/m²-24hr-atm
635 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
Melt Flow 25 g/10 min
25 g/10 min
(MVR) [cm³/10min]; ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 35.0 MPa
5080 psi
ISO 527-3
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ISO 527-3
Film Elongation at Break, MD 700 %
700 %
ISO 527-3
Film Elongation at Break, TD 700 %
700 %
ISO 527-3
Film Elongation at Yield, MD 15 %
15 %
ISO 527-3
Film Elongation at Yield, TD 15 %
15 %
ISO 527-3
Tensile Modulus 0.750 GPa
109 ksi
conditioned; ISO 527-1/-2
3.00 GPa
435 ksi
dry; ISO 527-1/-2
Coefficient of Friction, Dynamic 0.25
0.25
ISO 8295
Tear Strength 30.0 kN/m
171 pli
Trouser Tear resistance MD; ISO 6383-1
30.0 kN/m
171 pli
Trouser Tear resistance TD; ISO 6383-1
Elmendorf Tear Strength MD 1020 g
1020 g
ISO 6383-2
Elmendorf Tear Strength TD 1020 g
1020 g
ISO 6383-2
Film Tensile Strength at Break, MD 100 MPa
14500 psi
ISO 527-3
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Optical Properties Metric English Comments
Gloss 100 %
100 %
60°; ISO 2813
Descriptive Properties Value Comments
Food contact EU Requirements
FDA
Form Granules
Gelboflextest [holes/m²], EMS 800
Packaging Non oriented film
Oriented film
Paper coating
Tubes
Processing Blown Film Extrusion
Film Extrusion
Other Extrusion
Product Attributes Barrier Properties
High viscosity
Nucleated