Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.060 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.060 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Global MB-6366 High Density Polyethylene Description-high density for high quality, excellent creep & chemical resistanceApplications-drinking water pipe, industrial pipe, sewer pipeInformation provided by Global Polymers Corporation. |
|||
Melt Flow | 0.060 g/10 min @Load 2.16 kg |
0.060 g/10 min @Load 4.76 lb |
ASTM D 1238 |
Total 2287 HDPE Bimodal Film Resin Broad molecular weight distribution. Designed for die build-up sensitive equipmentApplications: T-shirt sacks, trash can liners, merchandise bags, deli wrapInformation provided provided by Total Pe.. |