Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.28 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.28 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 4 HM9455 F High Density Polyethylene EX4 is a high density polyethylene with 1-Butene as co monomer. It is high rigidity, low gel level, high drowdown, somewhat stiffer than EX 5.Applications: film extrusion, blending partner, refuse .. |
|||
Melt Flow | 0.28 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.28 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 5 HM 9450 F High Density Polyethylene EX5 is a high density polyethylene with 1-Butene as co monomer.Applications: film extrusion, counter bag, carrier bag, wrapping filmsInformation provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 0.28 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.28 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CARMELTECH™ QB 79 P Polypropylene Random Copolymer for Pressure Pipe CARMELTECH™ QB 79 P is a high molecular weight, low melt flow rate polypropylene random copolymer, especially designed for extrusion of pressure pipes and injection molding of fittings. This grade .. |