Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 100 g/10 min @Load 5.00 kg, Temperature 200 °C |
100 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Versaflex™ OM 9-801N Thermoplastic Elastomer (TPE) Versaflex™ OM 9-801N is designed for overmolding onto a wide variety of substrates including PC, ABS, PC/ABS, HIPS, PPO, acetal, acrylic and copolyester. - Bonds to a Variety Of Substrates - Rubber.. |
|||
Melt Flow | 100 g/10 min @Load 5.00 kg, Temperature 200 °C |
100 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE) Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established... |
|||
Melt Flow | 100 g/10 min @Load 5.00 kg, Temperature 200 °C |
100 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-9 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Excellent Grip with Matte, Rubbery Finish - P.. |
|||
Melt Flow | 100 g/10 min @Load 5.00 kg, Temperature 230 °C |
100 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® ESD 5400 PRE-ELEC ESD 5400 is a static dissipative thermoplastic compound based on poly-propylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 5400 is developed for t.. |
|||
Melt Flow | 100 g/10 min @Load 10.0 kg, Temperature 200 °C |
100 g/10 min @Load 22.0 lb, Temperature 392 °F |
ISO 1133 |
Kuraray SEPTON® S2002 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Melt Flow | 100 g/10 min @Load 5.00 kg, Temperature 260 °C |
100 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Styron EMERGEâ„¢ 7560 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ PC/ABS 7560 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the.. |
|||
Melt Flow | 100 g/10 min @Load 21.6 kg, Temperature 200 °C |
100 g/10 min @Load 47.6 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Sinelec CCB2765 General Purpose Polystyrene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Uses: Sheets Forms: Pellets Processing Method: Injection Method; Sheet Extrusion; Vac.. |