Material Notes:
PRE-ELEC ESD 5400 is a static dissipative thermoplastic compound based on poly-propylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 5400 is developed for tape and monofilament extrusion. The products made out of PRE-ELEC ESD 5400 are washable, reusable and recyclable. Surface resistance values of 109 ohms (EOS/ESD S11.11-1993, IEC 61340-5-1) can be achieved with optimum processing parameters.Typical applications include tapes and monofilaments for woven fabrics industry e.g. to produce ESD big bags. Test Specimen: TapeInformation provided by Premix Thermoplastics Inc.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
Melt Flow 26 g/10 min

@Load 2.15 kg,
Temperature 230 °C
26 g/10 min

@Load 4.74 lb,
Temperature 446 °F
ISO 1133
100 g/10 min

@Load 5.00 kg,
Temperature 230 °C
100 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Electrical Properties Metric English Comments
Surface Resistance <= 1.00e+10 ohm
<= 1.00e+10 ohm
9x Stretched Tape; ISO IEC 61340-5-1
Static Decay <= 2.0 sec
<= 2.0 sec
9x Stretched Tape; ISO IEC 61340-5-1
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions