Physical Properties Metric English Comments
Melt Flow 15.5 g/10 min

@Load 2.16 kg,
Temperature 250 °C
15.5 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
DuPont Performance Polymers Crastin® 6130 NC010 PBT  (Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
Melt Flow 15.5 g/10 min

@Load 6.60 kg,
Temperature 367 °C
15.5 g/10 min

@Load 14.6 lb,
Temperature 693 °F
ASTM D 1238
SABIC Innovative Plastics Ultem AUT230M PEI
Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are ..
Melt Flow 15.5 g/10 min

@Load 6.60 kg,
Temperature 367 °C
15.5 g/10 min

@Load 14.6 lb,
Temperature 693 °F
ASTM D 1238
SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific)
Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required...
Melt Flow 15.5 g/10 min

@Load 6.60 kg,
Temperature 367 °C
15.5 g/10 min

@Load 14.6 lb,
Temperature 693 °F
ASTM D 1238
SABIC Innovative Plastics Ultem AUT230M PEI (Europe-Africa-Middle East)
Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required...