Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name ULTEM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of 230 degC (SABIC Innovative Plastics method).This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D 792
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.65 %
0.65 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.75 %

@Temperature 23.0 °C
1.75 %

@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
on tensile bar; SABIC Method
0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 8.0 g/10 min

@Load 5.00 kg,
Temperature 360 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 680 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
15.5 g/10 min

@Load 6.60 kg,
Temperature 367 °C
15.5 g/10 min

@Load 14.6 lb,
Temperature 693 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 78.0 MPa
11300 psi
5 mm/min; ISO 527
96.0 MPa
13900 psi
Type I, 5 mm/min; ASTM D 638
Tensile Strength, Yield 95.0 MPa
13800 psi
5 mm/min; ISO 527
96.0 MPa
13900 psi
Type I, 5 mm/min; ASTM D 638
Elongation at Break 16.3 %
16.3 %
5 mm/min; ISO 527
25 %
25 %
Type I, 5 mm/min; ASTM D 638
Elongation at Yield 6.0 %
6.0 %
Type I, 5 mm/min; ASTM D 638
8.4 %
8.4 %
5 mm/min; ISO 527
Tensile Modulus 3.12 GPa
453 ksi
1 mm/min; ISO 527
3.51 GPa
509 ksi
5 mm/min; ASTM D 638
Flexural Yield Strength 123 MPa
17800 psi
2 mm/min; ISO 178
Flexural Modulus 3.07 GPa
445 ksi
2 mm/min; ISO 178
3.17 GPa
460 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 0.690 J/cm

@Temperature 23.0 °C
1.29 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
0.740 J/cm

@Temperature -30.0 °C
1.39 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
Izod Impact, Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
6.00 kJ/m²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 147 kJ/m²

@Temperature -30.0 °C
69.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
196 kJ/m²

@Temperature 23.0 °C
93.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Impact Test 33.0 J

@Temperature 23.0 °C
24.3 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 50.0 µm/m-°C

@Temperature -40.0 - 150 °C
27.8 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
50.0 µm/m-°C

@Temperature 23.0 - 150 °C
27.8 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C

@Temperature -40.0 - 150 °C
27.8 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
50.0 µm/m-°C

@Temperature 23.0 - 150 °C
27.8 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 237 °C

@Thickness 6.40 mm
459 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 228 °C
442 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
217 °C

@Thickness 3.20 mm
423 °F

@Thickness 0.126 in
unannealed; ASTM D 648
230 °C

@Thickness 6.40 mm
446 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Vicat Softening Point 240 °C
464 °F
Rate B/120; ISO 306
242 °C
468 °F
Rate B/50; ASTM D 1525
242 °C
468 °F
Rate B/50; ISO 306
Glass Transition Temp, Tg 247 °C
477 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C Passes
IEC 60695-10-2
Metallized Haze Onset, °C 230
SABIC Method