Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 25 g/10 min @Load 10.0 kg, Temperature 220 °C |
25 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 25 g/10 min @Load 10.0 kg, Temperature 220 °C |
25 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 220 °C |
25 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East) CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Europe-Africa-Middle East) UV stabilized, non-FR PC/ABS of excellent flow and impact performanceThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 25 g/10 min @Load 1.20 kg, Temperature 300 °C |
25 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXG173R PC This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 25 g/10 min @Load 1.20 kg, Temperature 300 °C |
25 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXM173R PC UV stabilized PC in special effects colors. Metallic and pearlescent additives. Color may affect performance.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 25 g/10 min @Load 1.20 kg, Temperature 300 °C |
25 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Melt Flow | 25 g/10 min @Load 1.20 kg, Temperature 300 °C |
25 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Asia Pacific) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 200 °C |
25 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G2703-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2703-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance and a low coefficient of friction. - Adhesion to Polypropylen.. |
|||
Melt Flow | 25 g/10 min @Load 21.6 kg, Temperature 190 °C |
25 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 2 HF 7750 M High Density Polyethylene EX2 is a high density polyethylene with 1-Butene as co monomer. It has good rigidity and medium molar mass. Applications: monofilaments, ropes, yarns.Information provided by Iran Petrochemical Com.. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1010A PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1010A PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 220 °C |
25 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1010FV PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 220 °C |
25 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1010FV PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 220 °C |
25 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1010FV PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1010K PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1010KM PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 220 °C |
25 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1010RV PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 220 °C |
25 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1010RV PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 220 °C |
25 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1010V PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 220 °C |
25 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 265 °C |
25 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East) VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 265 °C |
25 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Melt Flow | 25 g/10 min @Load 10.0 kg, Temperature 260 °C |
25 g/10 min @Load 22.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics LNP Thermocomp ML4351HF PC (Asia Pacific) LNP* Thermocomp* ML4351HF is a Light Reflecting Grade.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 25 g/10 min @Load 2.16 kg, Temperature 280 °C |
25 g/10 min @Load 4.76 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Melt Flow | 25 g/10 min @Load 21.6 kg, Temperature 190 °C |
25 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® FB3450 HDPE for Film Extrusion Borstar® FB3450 is a high density polyethylene. Borstar® FB3450 is well suited for multilayer coextruded films where higher stiffness and toughness than in standard LDPE and LLDPE is required. Ap.. |
|||
Melt Flow | 25 g/10 min @Load 21.6 kg, Temperature 190 °C |
25 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Total Lumicene® mPE BM359 SG Metallocene Medium Density High Gloss Blow Molding Resin Metallocene Medium Density High Gloss Blow Molding ResinCharacteristics:Outstanding glossGood flexibilityExcellent impact strengthGood ESCRUSP Class VI compliantFDA CompliantApplications:Coextruded .. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 230 °C |
25 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Borealis Xmod™ K65G3 30% Glass Fiber Reinforced Polypropylene Compound Xmod K65G3 is a 30% glass fiber reinforced grade intended for injection molding. Xmod K65G3 has been developed especially for the car industry, to be used UTB parts. Xmod K65G3 offers good balance.. |
|||
Melt Flow | 25 g/10 min @Load 2.16 kg, Temperature 280 °C |
25 g/10 min @Load 4.76 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |