Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® X37 ABS (Europe-Africa-Middle East) CYCOLAC X37 is the highest heat material available in the CYCOLAC range of materials and is widely recognized within the automotive industry as being the industry standard for high heat ABS. It comb.. |
|||
Melt Flow | 3.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® X37 ABS (Europe-Africa-Middle East) CYCOLAC X37 is the highest heat material available in the CYCOLAC range of materials and is widely recognized within the automotive industry as being the industry standard for high heat ABS. It comb.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers NPP 808 C2WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Melt Flow | 3.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Melt Flow | 3.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Melt Flow | 3.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer (Europe-Africa-Middle East) Transparent weatherable PC copolymer for blowmolding/extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7980-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylene - Rubbery Feel - Soft T.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg |
3.0 g/10 min @Load 11.0 lb |
ASTM D 1238 |
Total Finathene® 6006 HDPE, blow molding, pipe
(discontinued **) Finathene® 6006 is a high density polyethylene produced by the slurry loop low pressure polymerization process. Polymerization is conducted in the absence of any other comonomer. Finathene® 6006 h.. |
|||
Melt Flow | 3.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound
(discontinued **) Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238(G) |
LG Chemical ALPHALAC SH860 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Refrigerator Inner LinerCAS No. 9003-55-8Information provided by LG Chemical |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 (G) |
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Melt Flow | <= 3.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
<= 3.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
MTM Plastics Purpolen® PE Polyethylene Regrind Purpolen® is a sorted regrind material suited to the production of demanding end user products. Extrusion and injection molding grades are available in many colors. The basis of our Purpolen® .. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Melt Flow | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/ABS 8800 Availability: North AmericaForms: PelletsFeatures: High Impact Resistance and High Temperature StrengthProcessing Method: Profile ExtrusionInformation provided by TP Composites, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® TF-0956 HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg |
3.0 g/10 min @Load 11.0 lb |
ISO 1133 |
Total Lumicene® M 3410 EP HDPE Film, sheet FINACENE® M 3410 EP is a medium density metallocene based polyethylene resin. FINACENE® M 3410 EP is especially dedicated to film applications where a higher rigidity, good transparency and shrink.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Denka TP-802 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Melt Flow | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 3501 GF-30 Description: Reinforced Grade, 30%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 7600B Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 7602B Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers NPP 808 C2 TDS Polycarbonate Alloy, Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers SAN 268 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Asia Pacific) Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade Information provided by Samsung Cheil Industries. |