Material Notes:
FINACENE® M 3410 EP is a medium density metallocene based polyethylene resin. FINACENE® M 3410 EP is especially dedicated to film applications where a higher rigidity, good transparency and shrink properties are required, particularly in blend and coextrusion with LL/LDPE. FINACENE® M 3410 EP is suited for many applications in the field of consumer, industrial, food or hygiene packaging.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.934 g/cc
0.0337 lb/in³
ISO 1183
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
10% ant.; ASTM D1693
Melt Flow 0.90 g/10 min

@Load 2.16 kg
0.90 g/10 min

@Load 4.76 lb
ISO 1133
3.0 g/10 min

@Load 5.00 kg
3.0 g/10 min

@Load 11.0 lb
ISO 1133
High Load Melt Index 25 g/10 min

@Load 21.6 kg
25 g/10 min

@Load 47.6 lb
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 33.0 MPa
4790 psi
ISO 527
Tensile Strength, Yield 17.0 MPa
2470 psi
ISO 527
Elongation at Break 860 %
860 %
ISO 527
Elongation at Yield 12 %
12 %
ISO 527
Flexural Modulus 0.600 GPa
87.0 ksi
ASTM D 790
Dart Drop Test >= 50.0 g
>= 0.110 lb
20µm; ASTM D 1709
>= 100 g
>= 0.221 lb
40µm; ASTM D 1709
Thermal Properties Metric English Comments
Melting Point 124 °C
255 °F
DSC
Vicat Softening Point 122 °C
252 °F
ISO 306
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
40µm; ASTM D 1003
10 %
10 %
20µm; ASTM D 1003
Gloss 50 %
50 %
45 degrees, 20µm; ASTM D 2457
61 %
61 %
45 degrees, 40µm; ASTM D 2457
Descriptive Properties Value Comments
Food Status This material is formulated to comply with most requirements of the food packaging regulations