Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hybrid S464 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Borclean™ HC312BF Polypropylene Homopolymer for Capacitor Film Borclean HC312BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC312BF does not contain slip, antiblock, antist.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Borclean™ HC318BF Polypropylene Homopolymer for Capacitor Film Borclean HC318BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC318BF does not contain slip, antiblock, antist.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis HC101BF Polypropylene Homopolymer HC101BF is a polypropylene homopolymer. Applications: HC101BF has been developed especially for applications like: co-extrusion applications, print lamination, metallisable film, coated film, packa.. |
|||
Melt Flow | 3.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS 2501 Injection Molding Grade, Medium Impact, High Flow Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |