Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 37 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 37 g/10 min

@Load 10.0 kg,
Temperature 220 °C
37 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
LG Chemical HIPS 65IHE PS, Impact Modified
Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical
Melt Flow 37 g/10 min

@Load 5.00 kg,
Temperature 250 °C
37 g/10 min

@Load 11.0 lb,
Temperature 482 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Xenoy® XD549S PBT+PC (Europe-Africa-Middle East)
Xenoy XD549S is an automotive grade, designed for thin wall (2.5 mm.) direct gated exterior parts. The material has an excellent flow. Xenoy XD549S can be painted with primerless solvent or waterbas..
Melt Flow 37 g/10 min

@Load 1.20 kg,
Temperature 300 °C
37 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East)
XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C
Copyright © lookpolymers.com All Rights Reserved