Polymer Property : Melt Flow = 42 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 14 - 42 g/10 min

@Load 21.6 kg,
Temperature 190 °C
14 - 42 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Kazanorgsintez PE2NT 15-10 Linear Low Density Polyethylene
Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez
Melt Flow 14 - 42 g/10 min

@Load 21.6 kg,
Temperature 190 °C
14 - 42 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Kazanorgsintez PE2NT 15-5 Linear Low Density Polyethylene
Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez