Physical Properties Metric English Comments
Melt Flow 4.0 - 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 - 6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 2060S (60105) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 4.0 - 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 - 6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4020R (20405) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 3.0 - 6.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
3.0 - 6.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 20; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 4148B (484H2) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 4.0 - 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 - 6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4430S (30405) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 4.0 - 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 - 6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4435S (35405) Medium Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 4.0 - 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 - 6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4431S (30405) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 4.0 - 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 - 6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4436S (35405) Medium Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 3.5 - 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 - 6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 3501 SHF
Description: Super High FlowInformation provided by Diamond Polymers, Inc.
Melt Flow 4.0 - 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 - 6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Breplast Bretene SPF Thermoplastic Composite, 40% PP + 60% PE
Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A.
Copyright © lookpolymers.com All Rights Reserved