Physical Properties Metric English Comments
Melt Flow 9.6 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.6 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D 1238
SABIC Innovative Plastics Valox® 357 PBT
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 9.6 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.6 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East)
VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures.
Melt Flow 9.6 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.6 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Xenoy® 1731 PBT+PC
Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.
Melt Flow 9.6 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.6 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D 1238
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Europe-Africa-Middle East)
PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 9.6 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.6 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D 1238
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Asia Pacific)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 9.6 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.6 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D 1238
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 9.6 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.6 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D 1238
SABIC Innovative Plastics Xenoy® EXXY0112 PBT+PC (Asia Pacific)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 9.6 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.6 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D 1238
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Asia Pacific)
PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 9.6 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.6 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Diamond Polymers MS-170 Styrene Methyl Methacrylate Terpolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 9.6 g/10 min

@Load 5.00 kg,
Temperature 230 °C
9.6 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
DuPont Performance Polymers Hytrel® HTR5612BK TPC-ET  (Unverified Data**)
Hytrel® HTR5612BK HTR5612BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal durometer hardness of 54D, is pigmented black with fine particle size..