Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 0.0430 cc-mm/m²-24hr-atm | 0.109 cc-mil/100 in²-24hr-atm | |
Dow Saran® 867 PVDC SARAN® 867 barrier polymer, a copolymer of vinylidene chloride and vinyl chloride, designed for extrusion and coextrusion into barrier films used in flexible packaging applications for food. It is .. |