Oxygen Transmission 160 cc-mm/m²-24hr-atm
406 cc-mil/100 in²-24hr-atm
or 6400 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film. Clysar® EZS is a high slip version of EZ. Used where a premium product appearance ..