Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 1.50 cc-mm/m²-24hr-atm | 3.81 cc-mil/100 in²-24hr-atm | cc-mm/m²-24hr-atm. Based on 1 mil microfilm; ASTM D398555-81 |
Ashley Polymers Ashlene® 745 Nylon 6/69 A special copolymer ideal for blown and cast film coextrusion. This is a gel free resin with outstanding lot to lot consistency being produced by a continuous process. It has a lower melting point.. |
|||
Oxygen Transmission | 1.50 cc-mm/m²-24hr-atm | 3.81 cc-mil/100 in²-24hr-atm | cc-mm/m²-24hr-atm. Based on 1 mil microfilm; ASTM D398555-81 |
Ashley Polymers Ashlene® 746 Nylon 6/69 A special copolymer ideal for blown and cast film coextrusion. This is a gel free resin with outstanding lot to lot consistency being produced by a continuous process. It has a lower melting point.. |