Ashley Polymers Ashlene® 746 Nylon 6/69

Category Polymer , Thermoplastic , Nylon , Nylon 6/69
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 746 Nylon 6/69.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A special copolymer ideal for blown and cast film coextrusion. This is a gel free resin with outstanding lot to lot consistency being produced by a continuous process. It has a lower melting point and is less crystalline than standard Nylon 6.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Oxygen Transmission 1.50 cc-mm/m²-24hr-atm
3.81 cc-mil/100 in²-24hr-atm
cc-mm/m²-24hr-atm. Based on 1 mil microfilm; ASTM D398555-81
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.0 MPa
8700 psi
ATSM D638
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 362 %
362 %
ASTM D638
Tensile Modulus 0.335 GPa
48.6 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 196 °C
385 °F
ASTM D3418