Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 1.767 cc-mm/m²-24hr-atm | 4.488 cc-mil/100 in²-24hr-atm | 0% RH; ASTM D 3985 |
NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin HPs167-AB complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Che.. |