Oxygen Transmission 7.40 cc-mm/m²-24hr-atm

@Temperature 30.0 °C
18.8 cc-mil/100 in²-24hr-atm

@Temperature 86.0 °F
ASTM D3985
Eastman Embrace LV Copolyester for Extruded/Cast Film
Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo..