Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Embrace LV Copolyester for Extruded/Cast Film

Category Polymer , Film , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Embrace
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Embrace LV Copolyester for Extruded/Cast Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLower Shrink force than EmbraceGreat clarity and high glossSuper-high print definitionUltimate shrinkage of >70%Product Description: LV stands for LOW shrink force and VERSATILE shrink curve. Under normal extruder manufacturing conditions, this product maintains the same shrink characteristics expected from Eastman Embrace but has a 30% lower shrink force. Living up to its name, it demonstrates its versatility with its ability to be produced with up to a 40% reduction in shrink force versus the first generation Eastman Embrace copolyester with a shrink curve that is similar to both PVC and OPS while still maintaining ultimate shrinkage well above 70%. This versatility, not before possible with Eastman Embrace, is achieved by making changes to the extruders manufacturing process. Eastman Embrace LV emulates all visually satisfying attributes expected from the current Eastman Embrace such as high gloss and clarity. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®. This Product has been CRADLE TO CRADLE CERTIFIEDcm Silver.Information provided by Eastman.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D1505
Water Vapor Transmission 6.70 g/m²/day
0.431 g/100 in²/day
ASTM F1249
Oxygen Transmission 7.40 cc-mm/m²-24hr-atm

@Temperature 30.0 °C
18.8 cc-mil/100 in²-24hr-atm

@Temperature 86.0 °F
ASTM D3985
Viscosity Measurement 0.70
0.70
Inherent; EMN-A-AC-G-V-1
Thickness 250 microns
9.84 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 4.0 %
4.0 %
ASTM D882
Film Elongation at Break, TD 4.0 %
4.0 %
ASTM D882
Tensile Modulus 1.90 GPa
276 ksi
Film M.D.; ASTM D882
1.90 GPa
276 ksi
Film T.D.; ASTM D882
Tear Strength, Total 6.90 N
1.55 lb (f)
M.D., Elmendorf; ASTM D1922
8.50 N
1.91 lb (f)
T.D., Elmendorf; ASTM D1922
47.0 N
10.6 lb (f)
M.D., PPT; ASTM D2582
62.0 N
13.9 lb (f)
T.D., PPT; ASTM D2582
Tear Strength 34.0 kN/m
194 pli
M.D., Split Tear @ 254 mm/min; ASTM D1938
37.0 kN/m
211 pli
T.D., Split Tear @ 254 mm/min; ASTM D1938
Film Tensile Strength at Break, MD 51.0 MPa
7400 psi
ASTM D882
Film Tensile Strength at Break, TD 50.0 MPa
7250 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 69.0 °C
156 °F
ASTM D1525
Glass Transition Temp, Tg 69.0 °C
156 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 1.4 %
1.4 %
ASTM D1003
Gloss 161 %
161 %
at 60°; ASTM D2457
Transmission, Visible 89 %

@Thickness 0.250 mm
89 %

@Thickness 0.00984 in
Regular, Film; ASTM D1003
92 %

@Thickness 0.250 mm
92 %

@Thickness 0.00984 in
Total, Film; ASTM D1003
99 %

@Thickness 0.250 mm
99 %

@Thickness 0.00984 in
Transparency, Film; ASTM D1746
Users viewing this material also viewed the following: