Physical Properties Metric English Comments
Oxygen Transmission 80.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
203 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
3150 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2256 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Oxygen Transmission 80.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
203 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
3150 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2400 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Oxygen Transmission 80.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
203 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
800 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2400 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Oxygen Transmission 80.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
203 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
3150 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2405 MAS048 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Oxygen Transmission 80.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
203 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
800 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2405 MAS048 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Oxygen Transmission 80.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
203 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
3150 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2407 MAS070 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Oxygen Transmission 80.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
203 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
800 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2407 MAS070 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Oxygen Transmission 80.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
203 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
3150 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2407 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Oxygen Transmission 80.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
203 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
800 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2407 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..