Physical Properties Metric English Comments
Environmental Stress Crack Resistance 1.5 hour

@Pressure 2.50 MPa
1.5 hour

@Pressure 363 psi
ISO CD 16770
Iran Petrochemical (PCC) I3 HC 7260(THE) High Density Polyethylene
I3 (HC 7260) is a high density polyethylene with propylene as comonomer. The product has good impact strength, good stress cracking resistance, low warping and good flow ability as well as high dens..