Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) I3 HC 7260(THE) High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) I3 HC 7260(THE) High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
I3 (HC 7260) is a high density polyethylene with propylene as comonomer. The product has good impact strength, good stress cracking resistance, low warping and good flow ability as well as high density, hardness and stiffness. Applications: transport and stacking crates, bottle crates, engineering parts, closures.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.957 g/cc
0.0346 lb/in³
ISO 1183
Environmental Stress Crack Resistance 1.5 hour

@Pressure 2.50 MPa
1.5 hour

@Pressure 363 psi
ISO CD 16770
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
23 g/10 min

@Load 5.00 kg,
Temperature 190 °C
23 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ISO 868
Tensile Strength at Break 30.0 MPa
4350 psi
ISO 527
Tensile Strength, Yield 29.0 MPa
4210 psi
ISO 527
Elongation at Break >= 1000 %
>= 1000 %
ISO 527
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 72.0 °C
162 °F
ISO 306
Processing Properties Metric English Comments
Melt Temperature 138 °C
280 °F
200 - 280 °C
392 - 536 °F
Users viewing this material also viewed the following: