Physical Properties | Metric | English | Comments |
---|---|---|---|
Soluble Sulfates | 175 ppm | 175 ppm | dry weight basis |
Imerys KT Cast Slurryâ„¢ Kaolin KT Cast Slurry is a carefully controlled kaolin-water suspension formulated for use in ceramic operations.Information provided by Imerys |