Material Notes:
KT Cast Slurry is a carefully controlled kaolin-water suspension formulated for use in ceramic operations.Information provided by Imerys
Physical Properties Metric English Comments
Specific Gravity 1.757 g/cc
1.757 g/cc
as shipped
Solids Content 70 %
70 %
as shipped
Particle Size 0.50 µm
0.50 µm
20% finer than
1.0 µm
1.0 µm
39% finer than
2.0 µm
2.0 µm
55% finer than
5.0 µm
5.0 µm
76% finer than
10 µm
10 µm
87% finer than
20 µm
20 µm
96% finer than
Particle Mesh Size 80 Mesh
80 Mesh
0% retained
200 Mesh
200 Mesh
1.3% retained
325 Mesh
325 Mesh
3.5% retained
pH 4.5 - 6.5
4.5 - 6.5
Soluble Sulfates 175 ppm
175 ppm
dry weight basis
Component Elements Properties Metric English Comments
Al2O3 38.8 %
38.8 %
CaO 0.090 %
0.090 %
Fe2O3 0.50 %
0.50 %
K2O 0.10 %
0.10 %
Loss on Ignition(%) 13.7 %
13.7 %
MgO 0.030 %
0.030 %
Na2O 0.060 %
0.060 %
SiO2 45.1 %
45.1 %
TiO2 1.64 %
1.64 %