Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 7500 - 15000 cP | 7500 - 15000 cP | made with Brookfield's module of 4, with speed at 10 rpm at 25°C and apply a coefficient of 200; 540MA3C52 |
Solvay MIRAPOL® 550 SB Surfactant Description: Cationic polymer providing good wet/dry combability properties. Imparts smooth feel, anti-static, luster and detangling properties to the hair and silky feel to the skin. Stabilizes foa.. |
|||
Brookfield Viscosity | 8000 - 15000 cP | 8000 - 15000 cP | Base, RVF #6 spindle, 20 rpm @ 27°C |
3M Scotch-Weld™ DP-100 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP-100 is a two-part adhesives offering fast cure and machinability.Information provided by 3M |
|||
Brookfield Viscosity | 4000 - 15000 cP | 4000 - 15000 cP | RVT #4 sp @ 20 rpm |
3M Scotch-Weld™ TL72 Threadlocker Anaerobic Adhesive 3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening.. |
|||
Brookfield Viscosity | 11000 - 15000 cP | 11000 - 15000 cP | Base, RVF #7 spindle, 20 rpm |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Brookfield Viscosity | 7000 - 15000 cP | 7000 - 15000 cP | Accelerator, RFV #7 at 20 rpm |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |