Polymer Property : Brookfield Viscosity = 12.2 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 12.2 cP
12.2 cP
One Day, V20
PolyOne Geon™ 120 Series 129 Polyvinyl Chloride Homopolymer
The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging..